| Product Model | Polyimide Tubing |
Polymide Tubing is one of the materials under NASA’s space development program. It was originally used in space shuttles, military aircraft and other molded products. It has been applied in various fields and has the following advantages.
Tube is formed in one piece and the general spiral type is different from heating with no peeling phenomenon.
Thickness
It can be produced with an inner diameter of 0.127mm and a pipe wall of 0.025mm.
Special multiple structure, impact resistance, and bending resistance with no peeling or damage.
Various adhesives can be used, including alkaline and radioactive drugs. It is non-toxic, non-polluting and not harmful to the human body.
Convenient work
The pipe wall is solid and can be carried out smoothly during the casing operation, and the soldering operation can be carried out directly due to the heat resistance.
Cold and heat resistance
Withstanding temperature -269℃~+400℃
Specifications
| Material Property | Value |
|---|---|
| Elongation | 50% (nominal) |
| Thermal Range | −269 °C to 400 °C |
| Tensile Strength | 20,000 psi minimum |
| Hoop Stress | 11,000 psi minimum |
| Dielectric Strength | 4,000 V / 0.001″ thickness (min.) |
| Dielectric Constant | 3.4 |
| Radiation Resistance | 3.0 × 109 gamma dose (rad) |
| Coefficient of Thermal Expansion | 4.0 × 10−5 /°C |
| Coefficient of Thermal Conductivity | 35 × 10−5 cal/sec/cm²/°C/cm |
| Coefficient of Friction | 0.5 |

US polyimide tubing standard dimensions — nominal inside diameter (size # 25–36: 0.0179–0.0050″ / 0.455–0.127 mm) and nominal wall thickness (0.00100–0.00075″ / 0.025–0.019 mm).

Japan polyimide tubing standard dimensions (mm) — nominal inside diameter 0.20–2.00 mm with inside-diameter tolerance (−0.01 / +0.04…+0.09), standard wall thickness (0.04–0.08 mm) and standard outside diameter (0.28–2.12 mm).
Manufacturers: American Tubing, Japanese Tubing